Grade Name: CuZn28Sn1As
International Standard: EN 12164 CW706R
Other Names: Naval Brass, C46400 (American Standard), CZ111 (British Standard)
Excellent Corrosion Resistance: Particularly suitable for seawater and marine environments, with outstanding corrosion resistance.
Good Mechanical Properties: High strength and good ductility.
Anti-Biofouling: Excellent resistance to biofouling in marine environments.
Ease of Processing: Suitable for both hot and cold working, easy to form.
Wide Applications: Used in shipbuilding, marine engineering, heat exchangers, etc.
Product Form | Dimensions | Remarks |
Rods | Ø5mm - Ø200mm | Round, hexagonal, square rods |
Plates | Thickness: 0.5mm - 50mm | Width: 100mm - 600mm |
Tubes | Outer Diameter: Ø6mm - Ø150mm | Wall Thickness: 0.5mm - 10mm |
Wires | Ø0.1mm - Ø10mm | Coiled or straight |
Forgings | Customized as per customer requirements | Suitable for complex parts |
Element | Content (%) | Remarks |
Cu | 70.0 - 73.0 | Main component |
Zn | Balance | Main alloying element |
Sn | 0.8 - 1.2 | Improves corrosion resistance |
As | 0.02 - 0.10 | Enhances anti-biofouling properties |
Fe | ≤0.3 | Impurity |
Ni | ≤0.5 | Impurity |
Pb | ≤0.2 | Impurity |
Others | ≤0.2 | Impurity |
Property | Value | Remarks |
Density | 8.5 g/cm³ | - |
Melting Point | 900 - 925°C | - |
Thermal Conductivity | 120 W/(m·K) | 20°C |
Electrical Conductivity | 28% IACS | 20°C |
Thermal Expansion Coefficient | 20.2 × 10⁻⁶ /K | 20-300°C |
Specific Heat Capacity | 0.38 J/(g·K) | 20°C |
Property | Value | Remarks |
Tensile Strength | 450 - 600 MPa | - |
Yield Strength | 200 - 300 MPa | - |
Elongation | 20 - 35% | - |
Hardness | 80 - 130 HB | - |
Elastic Modulus | 100 - 110 GPa | - |
Excellent Corrosion Resistance: Particularly suitable for seawater and marine environments, with outstanding corrosion resistance.
Good Mechanical Properties: High strength and good ductility.
Anti-Biofouling: Excellent resistance to biofouling in marine environments.
Ease of Processing: Suitable for both hot and cold working, easy to form.
Shipbuilding: Used in ship components, propellers, etc.
Marine Engineering: Suitable for offshore platforms, seawater pipelines, etc.
Heat Exchangers: Used in seawater coolers, condensers, etc.
Chemical Equipment: Suitable for corrosion-resistant chemical equipment.
Power Industry: Used in seawater cooling systems, etc.
Hot and Cold Working: Be cautious of work hardening during cold working; hot working temperature should be between 600-800°C.
Machining: Use high-speed steel or carbide tools with moderate cutting speeds.
Welding: Good weldability; brazing or soft soldering is recommended.
Surface Treatment: Polishing, plating, etc., can enhance appearance and corrosion resistance.
Shipbuilding: Propellers, ship components, etc.
Marine Engineering: Offshore platforms, seawater pipelines, etc.
Heat Exchangers: Seawater coolers, condensers, etc.
Chemical Equipment: Corrosion-resistant chemical equipment.
Power Industry: Seawater cooling systems, etc.
A1: CuZn28Sn1As has excellent corrosion resistance, particularly suitable for seawater and marine environments.
A2: It has high strength and good ductility, making it suitable for high-strength mechanical parts.
A3: It has good weldability; brazing or soft soldering is recommended.
A4: It is widely used in shipbuilding, marine engineering, heat exchangers, and chemical equipment industries.
International Standard: EN 12164 CW706R
American Standard: ASTM B21 C46400
Japanese Standard: JIS H3250 C4621
Chinese Standard: GB/T 5231 HSn70-1
Tel:
E-mail:
Address:
No.1 Chengxi West Road, Cicheng, Ningbo, China